PRR-251

Mixture repair-reducing sulfate-resistant fine-grained

Properties:

  • high strength (not less than 45 MPa)
  • quick hardening (up to 3 hours)
  • excellent adhesion to concrete (at least 2.0 MPa)
  • microfiber reinforced
  • crack resistant
  • frost resistant
  • hydrophobic and vapor permeable
  • convenient and easy to use
  • resistant to oils and chemicals
  • high sulphate resistance
  • resistant to salt

Packing: 25 kg

Application
  • Application
  • Specifications
  • Documents
  • Reviews
  • Features

The PRR-251 mix is ​​intended for repair and restoration of concrete and reinforced concrete foundations, including objects of transport construction exposed loads RCC I, RCC II and
RCC III. Effective at repairing chips, voids, sinks, irregularities and other defects
surfaces of reinforced concrete and concrete substrates up to 30 mm thick with salt
sulfates impact. Do not use for leveling and repairing lightweight concrete foundations and foundations subject to significant mechanical effects.

The PRR-251 is an integral part of the system of  concrete restoration and protection . It is used when performing complex repairs of concrete and reinforced concrete structures caused by long-term operation or destruction under the influence of mechanical loads and corrosion processes – monolithic frame structures, retaining walls, tanks (including for wastewater).

Technical passport

CONCLUSION OF STATE SANITARY AND EPIDEMIOLOGICAL EXAMINATION ON DRY MIXTURES PC POLIPLAST LLC

CONCLUSION OF THE LABORATORY OF RADIOLOGICAL HYGIENE TM POLYPLAST | GLUE MIXTURES

Leave your review

There are no reviews yet.

Structurehigh strength cement mixture with mineral fillers, modifiers and reinforcing fibers
Appearancehomogeneous granular mixture gray without impurities
mixing ratio4.5-5.0 l of water per 25 kg of the dry mixture
While using mortarnot less than 30 minutes
Adhesion to concrete basenot less than 2.0 MPa
frost-resistancenot less than 75 cycles
Shrinkagenot more than 1.2 mm / m
Tensile strength in bending (after 28 days)not less than 5.0 MPa
The compressive strength (after 3 days)not less than 5.0 MPa
Compression strength (after 28 days)not less than 35.0 MPa
consumption mixture2.0 kg / m² at 1 mm layer thickness