PP-011 GRES

Adhesive mixture for porcelain tiles

Properties:

  • fixing ceramic tiles and tiles Gres
  • for vertical and horizontal surfaces
  • inside and outside buildings
  • high adhesion
  • moisture-resistant, frost-resistant
  • for systems "warm floor"

Packing: 25 kg

Application
  • Application
  • Specifications
  • Documents
  • Reviews
  • Features

The adhesive mixture PP-011 Gres is intended for facing vertical and horizontal bases with ceramic and porcelain stoneware (gres) tiles.

Suitable for slabs made of natural and artificial stone both inside and outside buildings. Place on horizontal bases tiles up to 450×450 mm, and up to 300×300 mm on vertical ones.

And also for laying tiles in systems “warm floor”.

The adhesive mixture is used on mineral non-deformable bases (concrete, cement, cement-lime, brick, plasterboard, etc.).

For fixing marble, especially light shades, it is recommended to use adhesive mixtures PP-015 BLANCO PP-016 BLANCO ULTRA Poliplast ™.

 

Technical passport

CONCLUSION OF STATE SANITARY AND EPIDEMIOLOGICAL EXAMINATION ON DRY MIXTURES PC POLIPLAST LLC

CONCLUSION OF THE LABORATORY OF RADIOLOGICAL HYGIENE TM POLYPLAST | GLUE MIXTURES

Leave your review

There are no reviews yet.

Compositiona mixture of cement with mineral aggregates and polymer modifiers

Appearance

uniform granular mixture of gray color without impurities

Aggregate size

no more than 0,8 mm

Mixing proportion

4.5-5.0 l of water per 25 kg (0.18-0.20 l of water per 1 kg) of dry mix

Layer thickness

2-10 mm

Air and base temperature during application

from +5 to +30 ° С

Expiration date from the moment of mixing

not less than 90 minutes

Open time

not less than 20 minutes

Adjustment time

 not less than 10 minutes

Time of possible technological movement

(joint stitching)

not less than 24 hours – for ceramics;

not less than 48 hours – for porcelain tile (Gres)

Base grip strength

not less than 0.8 MPa

Adhesion to the base after soaking in water

not less than 0.5 MPa
Adhesion to the base after alternate freezing and thawing (50 cycles)not less than 0.5 MPa

Adhesion to the base after temperature exposure (+70 ° C)

not less than 0.5 MPa

Compressive strength (after 28 days)

not less than 10.0 MPa

Hardened mortar operating temperature

from -30 to +70 °С
Dry mix consumptionfrom 2.0 kg / m2 (average 1.3 kg / m2 per 1 mm of layer thickness)

Where to buy

For technical advice and the purchase of our products, please contact us by phone or fill out the application form

or

Submit your application
Calculator Where To Buy